ASTM A240: grades
GradeAs printedYield strengthTensile strength
Lean duplex stainless steel 2101 (UNS S32101) A240plate, sheet and strip at least 450 MPa at least 650 MPa
Incoloy 800 (UNS N08800) A240plate, sheet and strip, with A480 250 to 690 MPa 590 to 771 MPa
Nitronic 60 stainless steel A240 345 to 393 MPa 655 to 717 MPa
Stainless steel 301 A240plate, sheet and strip 205 to 1,103 MPa 515 to 1,276 MPa
Duplex stainless steel 2205 A240plate, sheet and strip at least 450 MPa 655 to 965 MPa
Lean duplex stainless steel 2304 A240plate, sheet and strip at least 400 MPa 600 to 820 MPa
Stainless steel 304L A240 170 to 241 MPa 485 to 586 MPa
Stainless steel 310S A240plate, sheet and strip 205 to 290 MPa 500 to 750 MPa
AISI 321 stainless steel A240plate, sheet and strip 205 to 320 MPa 515 to 586 MPa
AISI 317L stainless steel A240plate, sheet and strip 200 to 260 MPa 500 to 700 MPa
Stainless steel 316 A240 193 to 213 MPa 480 to 620 MPa
AISI 347 stainless steel A240plate, sheet and strip 205 to 250 MPa 515 to 640 MPa
Stainless steel 409 A240plate, sheet and strip 170 to 255 MPa 380 to 560 MPa
Stainless steel 316L A240 170 to 290 MPa 485 to 558 MPa
Stainless steel 410 A240 205 to 1,089 MPa 448 to 1,331 MPa
Stainless steel 410S A240sheet, strip and plate 207 to 290 MPa 414 to 448 MPa
Stainless steel 430 A240Type 430 207 to 386 MPa 400 to 630 MPa
Stainless steel 444 A240plate, sheet and strip 275 to 350 MPa 415 to 600 MPa
Super-austenitic stainless steel 904L A240plate, sheet and strip 220 to 270 MPa 490 to 730 MPa
Stainless steel 304 A240 at least 205 MPa at least 515 MPa

Ranges run across the tempers and conditions each source reports, so a heat-treatable grade shows a wide range. Open a grade for each value with its condition and source.