Materials/Standards/ASTM A479

ASTM A479

astm-a479

Grades that cite ASTM A479

The grades in our database whose sources name ASTM A479. Each row shows how the source prints it, the product form the source ties to it where it says so, and the strength we hold for the grade. This is a finding aid, not the standard: the current text of ASTM A479 is sold by its publisher.

Product forms named by our sources: bar; bar and wire.

ASTM A479: grades
GradeAs printedYield strengthTensile strength
Nitronic 60 stainless steel A479 345 to 393 MPa 655 to 717 MPa
Duplex stainless steel 2205 A479bar at least 450 MPa 655 to 965 MPa
Stainless steel 304L A479bar and wire 170 to 241 MPa 485 to 586 MPa
Stainless steel 304 A479 at least 205 MPa at least 515 MPa

Ranges run across the tempers and conditions each source reports, so a heat-treatable grade shows a wide range. Open a grade for each value with its condition and source.

Often cited with