ASTM A276
astm-a276Grades that cite ASTM A276
The grades in our database whose sources name ASTM A276. Each row shows how the source prints it, the product form the source ties to it where it says so, and the strength we hold for the grade. This is a finding aid, not the standard: the current text of ASTM A276 is sold by its publisher.
Product forms named by our sources: bar; bar and shapes; bar and shape; bar and wire; listed specification for Type 420.
| Grade | As printed | Yield strength | Tensile strength |
|---|---|---|---|
| Nitronic 60 stainless steel | A276bar | 345 to 393 MPa | 655 to 717 MPa |
| Duplex stainless steel 2205 | A276bar and shapes | at least 450 MPa | 655 to 965 MPa |
| Lean duplex stainless steel 2304 | A276bar and shape | at least 400 MPa | 600 to 820 MPa |
| Stainless steel 304L | A276bar and wire | 170 to 241 MPa | 485 to 586 MPa |
| Stainless steel 316 | A276 | 193 to 213 MPa | 480 to 620 MPa |
| Stainless steel 316L | A276 | 170 to 290 MPa | 485 to 558 MPa |
| Stainless steel 410 | A276 Type 410 | 205 to 1,089 MPa | 448 to 1,331 MPa |
| Stainless steel 420 | A276listed specification for Type 420 | 355 to 1,311 MPa | 592 to 1,760 MPa |
| Stainless steel 431 | A276bar | 600 to 1,034 MPa | 800 to 1,379 MPa |
| Stainless steel 440C | A 276 | 1,896 MPa | 1,965 MPa |
| Stainless steel 444 | A276 | 275 to 350 MPa | 415 to 600 MPa |
| Stainless steel 304 | A276 | at least 205 MPa | at least 515 MPa |
| Martensitic stainless steel 13Cr-4Ni (UNS S41500) | A276 | at least 517 MPa | 700 to 1,100 MPa |
Ranges run across the tempers and conditions each source reports, so a heat-treatable grade shows a wide range. Open a grade for each value with its condition and source.
Often cited with
- ASTM A240: 20 grades
- ASTM A182: 6 grades
- ASTM A312: 4 grades
- ASTM A479: 4 grades
- EN 10088-3: 3 grades