ASTM B265: grades
GradeAs printedYield strengthTensile strength
Ti-6Al-4V B265Grade 5, sheet and plate 830 to 1,100 MPa no data
Commercially pure titanium with palladium, Grade 11 (UNS R52250) B265strip, sheet and plate 138 to 310 MPa 240 to 345 MPa
Commercially pure titanium, Grade 2 (UNS R50400) B265strip, sheet and plate 275 to 352 MPa 345 to 483 MPa
Titanium alloy Ti-6Al-4V ELI (Grade 23) B265sheet and plate, Grade 23 759 to 908 MPa 828 to 953 MPa
Commercially pure titanium, Grade 3 (UNS R50550) B265strip, sheet and plate 380 to 462 MPa 450 to 593 MPa
Commercially pure titanium, Grade 7 B265strip, sheet and plate at least 275 MPa 345 to 448 MPa
Titanium Grade 9, Ti-3Al-2.5V (UNS R56320) B265strip, sheet and plate 483 to 860 MPa 620 to 965 MPa

Ranges run across the tempers and conditions each source reports, so a heat-treatable grade shows a wide range. Open a grade for each value with its condition and source.